Fabric in the processing and taking the process, when subjected to external friction, such as friction is greater than the fiber strength or friction between the fibers or cohesion, the fiber ends will be pulled out to form a ring and fluff, the fabric surface to produce fluff So that the fabric lost luster. When the villi exposed to a certain length, the villi in a certain distance due to rubbing friction, repeated elongation and retraction and entangled into a ball, seriously affecting the appearance of the fabric surface. When the fabric surface of the pompon formation, due to the different fiber breaking strength, yarn twist, fabric structure and so on, some pompon after the formation of easy to fall off, and some easy to fall off, entanglement, and easy to filth , Affecting the quality of clothing taking. Cashmere fiber fine fineness, low strength, poor spinnability; Soybean protein fiber monofilament fine fineness, light weight, high strength, and acid and alkali resi...